Note when and where the crack appeared, then check the model design, resin condition, print conditions, washing and post-cure.
First, find out whether the part cracked during printing, at removal, after post-cure or in use. When and where it cracks helps you separate design, material, printing and post-processing causes.
1. Record when and where it cracked
Photograph where the crack starts and which way it runs. Mark thin edges, holes, corners, support contact points and areas loaded during assembly, and note the step where the problem first showed up.
2. Check the model and supports
Check wall thickness, sharp corners, holes and load direction, and look for supports that create local stress. If parts keep cracking in the same spot, check the design and orientation first.
3. Check the resin and print records
Confirm the product, lot, storage, mixing, environment and exposure settings. Contaminated resin, resin in poor condition or mismatched cure settings can all affect results.
4. Check washing and post-cure
Soaking too long, incomplete drying, the wrong cure settings or uneven heating can each create new problems. Run a controlled comparison: same model, every other condition held constant.
Related questions
Will more exposure fix brittle, cracking prints?
Not necessarily. Brittleness can come from the design, the resin’s condition or post-processing. Raising exposure blindly can also cause dimensional and surface problems.
If parts crack only after post-cure, what should I check first?
First check washing and drying, the curing unit, temperature, time and part placement. Then look at internal stress and weak points in the part design.
This article describes a general method. For specific settings, follow the current TDS, SDS and IFU for the product and your own test prints.