Definitions, units and test methods for the 13 terms you’ll see most often on LEYI technical data sheets.
ShrinkageShrinkage
The percentage of volume a photopolymer resin loses as it cures from liquid to solid. The lower the shrinkage, the closer the printed part stays to the design dimensions.
Flexural strengthFlexural Strength
The maximum stress a specimen withstands under bending before it breaks or reaches a specified deflection. Reported in MPa and tested to ISO 178, it is the main strength metric for crown and bridge resins and denture base resins.
Elongation at breakElongation at Break
The increase in length of a specimen at the point of fracture, divided by its original gauge length and expressed as a percentage. Tested to ISO 527-2, it indicates how tough or ductile a material is.
Shore hardnessShore Hardness
Hardness measured by how far a standardized indenter penetrates the material under specified conditions, tested to ISO 868. Soft materials use the Shore A scale and rigid resins use Shore D. Values on the two scales can’t be compared directly.
BiocompatibilityBiocompatibility
A material’s ability to contact human tissue without causing an unacceptable adverse reaction. It is evaluated under the ISO 10993 series; common endpoints include cytotoxicity, sensitization and irritation.
Heat deflection temperature (HDT)HDT
The temperature at which a specimen under a specified bending load, heated at a constant rate, reaches a specified deflection. Tested to ISO 75-2, it describes a material’s short-term heat resistance.
405 nm photopolymerization405 nm Photopolymerization
Curing a resin with 405 nm light to start polymerization. 405 nm is the most common light-source wavelength in dental LCD and DLP printers.
Post-curePost-curing
UV exposure applied after printed parts are washed and dried. It polymerizes residual monomer so the part reaches its specified mechanical properties and dimensional stability.
ViscosityViscosity
A measure of a liquid’s resistance to flow, in mPa·s (numerically equal to cP, or cps). Resin viscosity rises as temperature drops, and resin that is too viscous levels poorly in the vat and lowers print success rates.
Flexural modulusFlexural Modulus
The ratio of stress to strain in the elastic region of a flexural test. Reported in MPa and tested to ISO 178, it describes a material’s stiffness.
Tensile strengthTensile Strength
The maximum stress a specimen withstands in a tensile test. Reported in MPa and tested to ISO 527-2.
Notched impact strengthNotched Izod Impact
The energy absorbed when a notched specimen is broken by a pendulum impact, divided by the specimen thickness. Reported in J/m and tested to ISO 180 (Izod), it describes a material’s resistance to impact fracture.
Tear strengthTear Strength
The force needed to tear a specimen, divided by its thickness. Reported in kN/m and tested to ISO 34-1, it is the key metric for soft resins such as gingiva mask materials.
For the values of each resin, see Resin comparison chart.