Knowledge base

What should I check when prints come out sticky?

First find out whether the tackiness is local or overall, then check washing, drying, post-cure, resin condition and print conditions one by one.

Quick answer

A sticky surface usually points to uncured resin left on the part, spent wash solvent, incomplete drying or the wrong post-cure conditions. Don’t keep extending exposure. Keep the failed part as is and start with your post-processing records.

1. Find where the part is sticky

Note whether the tackiness covers the whole surface, downward-facing areas, holes and grooves, or the areas near supports. Local and overall tackiness have different causes, so photograph the part and keep it.

2. Check washing and drying first

  • Do the wash solvent, number of washes and wash time match the product requirements?
  • Is the wash solvent visibly contaminated?
  • Is liquid resin still trapped in grooves or holes?
  • Was the part completely dry before post-cure?

3. Then verify post-cure

Confirm that the curing unit, light spectrum, time, temperature, part placement and flipping match the resin you’re using. Don’t rely on settings from another resin or another curing unit.

4. Finally, check printing and resin condition

If your post-processing records look normal, check the resin lot, storage, mixing, exposure and environment. Change one variable at a time and reprint a small test part each time.

5. When to stop using the resin

Stop using the resin and contact technical support if you can’t confirm its source or storage, if you see contamination or unusual clumping, if problems persist across the same lot, or if the parts are for safety-critical or medical use.

Related questions

Can I just extend post-cure time when a surface is sticky?

Not before you check washing and drying. First make sure no liquid resin remains on the surface, then confirm the cure conditions specified for the product.

What could cause stickiness only inside grooves?

Common causes are resin that didn’t drain, incomplete washing, insufficient drying or light that was blocked during curing. Check each one at the affected area.

This article describes a general method. For specific settings, follow the current TDS, SDS and IFU for the product and your own test prints.

More in this category

Having an issue? Note the symptom, printer model and resin model, then Contact support.