Clear aligners are thermoformed from plastic sheet over 3D printed models, so the accuracy and surface quality of the model directly decide how well the aligner fits and how clear it looks. Fit depends on a model that prints true to the design and holds its shape during thermoforming, which calls for a resin with low shrinkage, good heat resistance and high strength. Appearance depends on a model with crisp detail and a matte, smooth, scratch-resistant surface. This article walks through the aligner workflow, what the model resin has to deliver and how to measure model accuracy. Using LEYI DMH02 Ortho Model Resin as an example, it gives property data and before-and-after thermoforming scan comparisons, then covers model design, printing, post-processing and troubleshooting. DMH02 reaches a heat deflection temperature of up to 70°C and a flexural modulus of up to 2800 MPa. In two model sets, more than 95% of measured points stayed within ±0.1 mm after thermoforming, with a best result of 99.75%.
1. Orthodontics and clear aligner therapy
Orthodontic treatment applies steady, controlled forces that move teeth through the alveolar bone to correct crowding, spacing, deep bite, crossbite and other malocclusions. Conventional fixed appliances use brackets and archwires. Clear aligner therapy uses a series of clear, removable trays instead. Each tray moves the teeth a small amount, and the patient wears them in sequence until the teeth reach the planned position. Because aligners are nearly invisible, removable and easy to keep clean, they are now a common choice for adult patients.
2. How clear aligners are made from 3D printed models
Most clear aligners are thermoformed. The workflow is: capture the patient’s 3D dentition data; the orthodontist plans treatment, exports the dentition for each stage and generates model STL files; the models are printed on a photopolymer printer, then washed and post-cured; plastic sheet is thermoformed over each model; the aligner is trimmed along the gingival line; and the aligner is cleaned, disinfected and packaged (Figure 1).
Depending on case complexity, a single case typically needs 20–60 aligners. Each aligner is formed on its own stage model, and consecutive stage models differ only slightly. Any error in the model transfers straight to the aligner. This article covers models for thermoforming only, not direct-printed aligners.

3. What aligner production demands from a 3D printed model
An aligner has to fit first and look good second. Each of those goals maps to specific model properties.
3.1 Fit: print accuracy and thermoforming accuracy
Aligner accuracy depends on how the model performs at two stages: the error introduced during printing and the deformation introduced during thermoforming.
3.1.1 Print accuracy
Print accuracy is how closely the finished model, after printing, washing and post-cure, matches the design data. It comes down to three factors:
- Low resin shrinkage. Photopolymer resins shrink as they polymerize. The more they shrink, and the less evenly, the more likely the model is to come out off-size or warped.
- An accurate printer. Optical resolution, light-source uniformity and build platform leveling determine the model’s dimensional accuracy and detail reproduction.
- The right print settings. Layer thickness and per-layer exposure time must match the resin and the printer. Overexposure makes the model oversized and blurs detail. Underexposure leaves the model undercured with weak layer bonding. See Section 6 for DMH02 recommended settings.
3.1.2 Thermoforming accuracy
During thermoforming, the heated, softened sheet is pressed onto the model by positive pressure or vacuum. As the sheet cools it shrinks and clamps down on the model, and removing the aligner then pulls on the model. Thin gingival margins, attachments and interproximal undercuts are the areas most likely to soften and distort or chip (Figure 2).
That is why a thermoforming model needs good heat resistance (measured as heat deflection temperature) and high strength and stiffness (measured as flexural modulus and flexural strength), so it deforms as little as possible under heat and load. DMH02 reaches an HDT of up to 70°C and a flexural modulus of up to 2800 MPa (see Section 5). Model deformation can be quantified by 3D scan comparison (see Section 4).
Note that thermoforming machines typically heat the sheet to 150–190°C and hold forming pressure for 15–25 s. The heated sheet is moved onto the model, where it conforms and cools quickly. The model surface is heated only briefly and stays far cooler than the sheet’s heating temperature.

3.2 Appearance: surface texture and clarity
A good-looking aligner has clean surface texture and high clarity. Clarity depends mostly on the sheet material, but the model’s surface also transfers to the inside of the aligner. Layer lines, scratches and support marks all make the aligner look less clear.
For the model, that means crisp detail and a matte, smooth, scratch-resistant surface:
- Matte: A glossy, reflective model can leave marks on the aligner after thermoforming. Glossy surfaces are also hard for 3D scanners to capture, which makes complete scan data difficult to get and undermines the accuracy checks described in Section 4.
- Smooth and scratch-resistant: A smooth, scratch-resistant surface releases the aligner more easily, which reduces sheet distortion and tearing from difficult removal and lowers the aligner reject rate. Test scratch resistance directly with a suitable tool or a fingernail. Shore hardness does not fully reflect scratch resistance and should not be used as the only criterion.
LEYI DMH02 is formulated to give models a matte, smooth surface with improved scratch resistance.
4. How to measure model accuracy
Model accuracy is usually measured by 3D scan comparison, the method most major aligner manufacturers use. It covers three checks (Figure 3):
- Print accuracy: Scan the model after printing, washing and post-cure and compare it with the design data. This shows the error introduced by printing.
- Thermoforming accuracy: Scan the same model before and after thermoforming and compare the two scans. This shows the deformation introduced by thermoforming.
- Final deformation: Compare the model after thermoforming with the original design data. This shows the total error accumulated across the whole workflow.
The main metric is the percentage of measured points within ±0.1 mm tolerance (comparison accuracy), with root mean square error (RMS) as a secondary metric. The higher the comparison accuracy, the closer the model is to the reference. Print accuracy alone tells you nothing about how the model deforms during thermoforming, so evaluate each stage separately.

5. Recommended: LEYI DMH02 Ortho Model Resin
DMH02 is LEYI’s gray ortho model resin for printing the models used in clear aligner thermoforming. It works with 385–405 nm DLP and LCD printers.
5.1 Properties and print settings
Table 1. DMH02 properties and print settings
| Property | DMH02 | Test method / notes |
|---|---|---|
| Color | Gray | Shade guide, visual |
| Viscosity (25°C) | 500–800 mPa·s | Viscometer |
| Heat deflection temperature (HDT) | 63–70°C | ISO 75-2, 0.45 MPa |
| Flexural modulus | 2400–2800 MPa | ISO 178 |
| Flexural strength | 60–70 MPa | ISO 178 |
| Tensile strength | 52–62 MPa | ISO 527-2 |
| Elongation at break | 5–10% | ISO 527-2 |
| Notched impact strength | 12–18 J/m | ISO 180 |
| Shore hardness | 83–87D | ISO 868 |
| Compatible printers | 385–405 nm DLP and LCD printers | Broad printer compatibility |
Source: LEYI DMH02 Technical Data Sheet (TDS). The latest TDS takes precedence.
5.2 Accuracy before and after thermoforming
Test conditions: Geomagic Control 3D deviation analysis software; best-fit alignment; tolerance ±0.1 mm; 2 sample sets. This test measures thermoforming accuracy as defined in Section 4, that is, the deformation introduced by thermoforming. Results are in Table 2.
Table 2. 3D deviation of DMH02 models before vs. after thermoforming
| Metric | Sample 1 | Sample 2 |
|---|---|---|
| Max. model length | 62.81 mm | 62.77 mm |
| Points compared | 27,335 | 27,862 |
| Accuracy within ±0.1 mm | 99.75% | 96.64% |
| Out of tolerance (+ / −) | 0.14% / 0.11% | 0.93% / 2.43% |
| Root mean square error (RMS) | 0.036 mm | 0.059 mm |
| Mean deviation (+ / −) | +0.027 / −0.027 mm | +0.036 / −0.046 mm |
| Standard deviation | 0.035 mm | 0.059 mm |
| Max. deviation (+ / −) | +0.237 / −0.119 mm | +0.393 / −0.515 mm |
Source: LEYI DMH02 before/after thermoforming 3D comparison report (Geomagic Control).
Comparison accuracy within ±0.1 mm before vs. after thermoforming was 99.75% and 96.64% for the two samples, both above 95%. RMS was 0.036 mm and 0.059 mm, which shows that thermoforming introduced little deformation. The deviation color maps show nearly the entire dental arch of Sample 1 within tolerance. In Sample 2, out-of-tolerance points are concentrated in a few local areas, mainly the distal surfaces of the last molars and the incisal edges of the anterior teeth (Figures 4 and 5).


These results reflect one specific set of print and thermoforming conditions. Results with other printers, sheet materials and thermoforming settings need to be verified separately. We recommend spot-checking with your own equipment and sheet material using the method in Section 4.
5.3 Other options
- DMH01 HT100°C Model Resin: HDT of 80–110°C (ISO 75-2). Use it with sheet materials that thermoform at higher temperatures, or when trial aligners show rounded gingival margins or distorted attachments. It also works for removable denture models.
- DMW04 Washable Model Resin: Wash off residual resin with plain water after printing. No ethanol, IPA or other flammable solvents needed.
6. Model design, printing and post-processing
6.1 Model design before printing
Some thermoforming defects start in the model design and are best fixed before printing (Figure 6):
- Block out undercuts: Fill deep undercuts in your design software so the aligner comes off in a single direction without pulling on the gingival margin.
- Labels: Place patient and stage IDs outside the area the sheet covers so the model can be traced through thermoforming, trimming and archiving.
- Wall thickness for hollow models: Print ortho models hollow. Solid models waste resin and add cost, and they are also more likely to warp during printing, which reduces accuracy. Walls that are too thin can crack under thermoforming. For hollow DMH02 models, the recommended wall thickness is 2 mm, within a range of 1.7–2.3 mm.
- Orientation and supports: Ortho models have a flat base, so you can usually print them flat on the build platform with no supports, which gives the best accuracy. To fit more models per print, angle them and add supports. Place supports on the base, outside the area the sheet covers, and keep them off the teeth and gingival line so support marks don’t transfer to the inside of the aligner (Figure 7).


6.2 Printing and post-processing
- Print environment: Keep room temperature at 23–25°C. When it is too cold, resin viscosity rises and print failures increase.
- Print settings: Recommended layer thickness 0.05 mm, 3–7 bottom layers, 3–4.5 s exposure per layer and 20–30 s bottom exposure. Fine-tune to your printer’s light output. After switching printers, print a single model and measure it before running full batches.
- Wash: Wash in IPA in an ultrasonic cleaner for 1.5 min, blow dry with compressed air, then wash for 1 min in fresh IPA. Uncured resin collects mainly in interproximal gaps, around attachments and inside hollow models (Figure 8). Blow out remaining liquid with compressed air after washing. If residue remains, rewash in clean IPA. Avoid long soaks, which can soften the surface.
- Drying: Blow the model dry with an air gun and let the alcohol evaporate completely before post-curing.
- Post-cure: UV post-cure for 5 min in a medium-power curing unit. Post-cure leaves the surface dry and fully cured and helps improve heat resistance. An incomplete post-cure reduces the model’s shape stability during thermoforming.


6.3 Thermoforming and aligner removal
Thermoforming settings depend mainly on the sheet type, sheet thickness and thermoforming machine. Machines typically heat the sheet to 150–190°C and hold forming pressure for 15–25 s; follow the sheet and equipment instructions. When you first switch to DMH02, form one trial aligner with your usual settings and check the gingival margins, attachments and removal. If everything looks right, move to production.
Let the sheet cool completely before removing it from the model. Removing it while still warm can distort the aligner. If removal is difficult, find where it is catching first. Common causes are incomplete undercut blockout or residual resin on the model sticking to the sheet. After removal, trim along the gingival line, finish the edges and inspect for bubbles, wrinkles, tears and attachment shape, then clean, disinfect and package. Archive each model and aligner under matching IDs for traceability.

7. Troubleshooting
Table 3. Common ortho model problems, causes and fixes
| Problem | Possible cause | Fix |
|---|---|---|
| Failed print or damaged model | Room temperature too low; poorly placed supports; resin degraded or too viscous from improper storage (failure risk rises above 1500 mPa·s) | Keep room temperature at 23–25°C; check support placement and density; if the resin is too viscous, warm the resin in the vat to above 30°C to lower viscosity |
| Rounded gingival margins or distorted attachments after thermoforming | Model softened by heat | Check that model walls are not too thin; confirm full post-cure; shorten heating time within the sheet’s allowed range; if needed, switch to heat-resistant DMH01 |
| Sheet sticks to the model, hard to remove | Undercuts too deep; residual resin on the surface, or post-cured before fully dry | Block out undercuts at the design stage; review the wash and drying steps |
| Gingival margin chips during removal | Aligner forced off while caught on an undercut; thin edges too weak | Find where it is catching before removing; block out undercuts; increase model wall thickness |
| Hollow model cracks during thermoforming | Walls too thin | Increase wall thickness to the recommended range |
| Fine lines on the inside of the aligner | Visible layer lines on the model | Reduce layer thickness; change print orientation; check that the printer’s mechanical motion is stable |
| Aligner fits too tight or too loose | Model print error or thermoforming deformation | Evaluate print accuracy and thermoforming accuracy separately to find the source of the error |
Related questions
Does a more heat-resistant resin make aligners more accurate?
It reduces model deformation during thermoforming, which cuts the error introduced at that stage. Final aligner accuracy, however, also depends on scanning, design, print accuracy, the sheet material, thermoforming settings, and trimming and finishing.
Can DMH02 be used to print aligners directly?
No. DMH02 is a model resin. Models do not go in the mouth, and DMH02 is not for direct-printed aligners. Direct printing of aligners is a recent process, and it still lacks sufficient clinical evidence on consistent treatment results and on safety for long-term intraoral use. Most aligners today are still thermoformed. If you want to try direct printing, use a dedicated material with the appropriate medical device registration, and have the orthodontist assess the risks.
What are my options if I don’t want to wash in alcohol?
Use LEYI DMW04 Washable Model Resin. After printing, residual resin washes off with plain water.
Which resin should I choose for higher-temperature thermoforming?
Consider LEYI DMH01 heat-resistant model resin (HDT 80–110°C, ISO 75-2). As with any resin, run trial aligners with your actual sheet material and thermoforming settings before adopting it.
This article describes general practice for thermoforming models. For specific settings, follow the latest product TDS, SDS and IFU and your own trial results. Model resin is for making models only; clinical use of aligners is decided by the orthodontist.
References LEYI DMH02 Technical Data Sheet (TDS); LEYI DMH02 before/after thermoforming 3D comparison report (Geomagic Control); ISO 75-2, ISO 178, ISO 527-2, ISO 180, ISO 868
Related resins
Having an issue? Note the symptom, printer model and resin model, then Contact support.